Warning: use of muriatic acid and LYE used in this video and should only be done in well ventilated area with full face,hand and eye protection. Click the “show more” to see full recipe.
2 Gal. distilled water
4oz zinc powder
6oz Lye Crystals
1 zinc anode (any size)
8 packets of Sweet n Low